Dental Alloy
• Ni-Cr-Mo alloy for quality dental restorations
• Biocompatible (biocompatibility certified)
• Density: 8.4 g/cm3
• Melting temperature : 1350C
• Vickers Hardness: 200 HV
• Composition (wt%): Ni 64-67, Cr 20-24,
Mo 8-11, Si 2, Nb, Fe, Al.
• Oxide formed is very light and easy to remove
• Easy to cast
• Easy to finish
• Biocompatible (biocompatibility certified)
• Density: 8.4 g/cm3
• Melting temperature : 1350C
• Vickers Hardness: 200 HV
• Composition (wt%): Ni 64-67, Cr 20-24,
Mo 8-11, Si 2, Nb, Fe, Al.
• Oxide formed is very light and easy to remove
• Easy to cast
• Easy to finish